Title: | Low permittivity SrCuSi4O10-LMZBS glass composite for LTCC applications |
Authors: | Manu, K M Anjana, P S Sebastian, M T |
Keywords: | Silicates Thermal-expansion Microwave dielectric-properties Densification LTCC Dielectric loss Relative permittivity Ceramics |
Issue Date: | 2011 |
Publisher: | Elsevier |
Citation: | Materials Letters 65(3): 565-567; 15 Feb 2011 |
Abstract: | The tetragonal gillespite type SrCuSi4O10 (SCS) was prepared by the conventional solid-state ceramic route. The SCS sintered at 1100 degrees C/6 h showed epsilon(r) = 4.0 and tan delta =1.1 x 10(-3) at 5 GHz. The SCS has poor sinterability and the addition of lithium magnesium zinc borosilicate glass (20: Li2O, 20: MgO, 20: ZnO, 20: B2O3, 20: SiO2) lowered the sintering temperature and improved densification. The SCS ceramic with 5 wt.% LMZBS glass sintered at 900 degrees C has epsilon(r) = 5.0 and tan delta = 1.9 x 10(-3) at 5 GHz. The composite is chemically compatible with the common electrode material silver. |
URI: | http://ir.niist.res.in:8080/jspui/handle/123456789/761 |
ISSN: | 0167-577X |
Appears in Collections: | 2011 |
Files in This Item:
File | Description | Size | Format | |
---|---|---|---|---|
2011_ 0061.pdf Restricted Access | 350.45 kB | Adobe PDF | View/Open Request a copy |
Items in DSpace are protected by copyright, with all rights reserved, unless otherwise indicated.