Biju, A; Shabna, R; Sarun, P M; Vinu, S; Syamaprasad, U
(Wiley, 2010)
Resistivity measurements in the temperature range (64-300 K) were used to study the metal-insulator transition (MIT) driven by a change in the carrier concentration of the Bi(1.7)Pb(0.4)Sr(2)Ca(1.1)Cu(2.1)O(y) [(Bi,Pb)-2212] ...