dc.contributor.author | Anjana, P S | |
dc.contributor.author | Joseph, T | |
dc.contributor.author | Sebastian, M T | |
dc.date.accessioned | 2014-06-25T11:18:25Z | |
dc.date.available | 2014-06-25T11:18:25Z | |
dc.date.issued | 2010 | |
dc.identifier.citation | Ceramics International 36(5):1535-1540;Jul 2010 | en_US |
dc.identifier.issn | 0272-8842 | |
dc.identifier.uri | http://ir.niist.res.in:8080/jspui/handle/123456789/1550 | |
dc.description.abstract | Ce-2(WO4)(3) ceramics have been synthesized by the conventional solid-state ceramic route. Ce-2(WO4)(3) ceramics sintered at 1000 degrees C exhibited epsilon(r) = 12.4, Qxf = 10,500 GHz (at 4.8 GHz) and tau(f) = -39 ppm/degrees C. The effects of B4O3, ZnO-B2O3, BaO-B2O3-SiO2, ZnO-B2O3-SiO2 and PbO-B2O3-SiO2 glasses on the sintering temperature and microwave dielectric properties of Ce-2(WO4)(3) were investigated. The Ce-2(WO4)(3) + 0.2 wt% ZBS sintered at 900 degrees C/4 h has epsilon(r) = 13.7, Qxf = 20,200 GHz and tau(f) = -25 ppm/degrees C. | en_US |
dc.language.iso | en | en_US |
dc.publisher | Elsevier | en_US |
dc.subject | Powders: solid state reaction | en_US |
dc.subject | Electron microscopy | en_US |
dc.subject | Dielectric properties | en_US |
dc.subject | Cofired ceramics | en_US |
dc.subject | Substrates | en_US |
dc.title | Low temperature sintering and microwave dielectric properties of Ce-2(WO4)(3) ceramics | en_US |
dc.type | Article | en_US |