  • SeethaLekshmi, S; Kiran, M S R N; Ramamurty, U; Varughese, S (Wiley, 2019-01-10)
    Comprehension of the nanomechanical response of crystalline materials requires the understanding of the elastic and plastic deformation mechanisms in terms of the underlying crystal structures. Nanoindentation data were ...