| dc.contributor.author | Manu, K M | |
| dc.contributor.author | Anjana, P S | |
| dc.contributor.author | Sebastian, M T | |
| dc.date.accessioned | 2013-11-19T05:01:02Z | |
| dc.date.available | 2013-11-19T05:01:02Z | |
| dc.date.issued | 2011 | |
| dc.identifier.citation | Materials Letters 65(3): 565-567; 15 Feb 2011 | en_US | 
| dc.identifier.issn | 0167-577X | |
| dc.identifier.uri | http://ir.niist.res.in:8080/jspui/handle/123456789/761 | |
| dc.description.abstract | The tetragonal gillespite type SrCuSi4O10 (SCS) was prepared by the conventional solid-state ceramic route. The SCS sintered at 1100 degrees C/6 h showed epsilon(r) = 4.0 and tan delta =1.1 x 10(-3) at 5 GHz. The SCS has poor sinterability and the addition of lithium magnesium zinc borosilicate glass (20: Li2O, 20: MgO, 20: ZnO, 20: B2O3, 20: SiO2) lowered the sintering temperature and improved densification. The SCS ceramic with 5 wt.% LMZBS glass sintered at 900 degrees C has epsilon(r) = 5.0 and tan delta = 1.9 x 10(-3) at 5 GHz. The composite is chemically compatible with the common electrode material silver. | en_US | 
| dc.language.iso | en | en_US | 
| dc.publisher | Elsevier | en_US | 
| dc.subject | Silicates | en_US | 
| dc.subject | Thermal-expansion | en_US | 
| dc.subject | Microwave dielectric-properties | en_US | 
| dc.subject | Densification | en_US | 
| dc.subject | LTCC | en_US | 
| dc.subject | Dielectric loss | en_US | 
| dc.subject | Relative permittivity | en_US | 
| dc.subject | Ceramics | en_US | 
| dc.title | Low permittivity SrCuSi4O10-LMZBS glass composite for LTCC applications | en_US | 
| dc.type | Article | en_US |